latheBy Kezuriba Editorial Team

How to hold thin-walled parts on a lathe and prevent deformation: three-jaw triangular distortion, soft jaws, sector jaws, clamping force calculation, and measurement

It was perfectly round on the lathe, but it came off shaped like a rice ball... Let's rethink the gripping force and how the jaws touch!

Chips, the Kezuriba mascot
How to hold thin-walled parts on a lathe and prevent deformation: three-jaw triangular distortion, soft jaws, sector jaws, clamping force calculation, and measurement

When you grip a thin tube or ring in a 3-jaw chuck and turn it, it may cut perfectly round on the lathe, but once released it takes on a rice-ball-like three-lobe shape. The cause is that the part is cut while it is distorted by the gripping force. For example, if you grip an aluminum ring of φ100 OD and 2 mm wall with point contact in a 3-jaw chuck at a total of 300 N (about 30 kgf), the calculation shows a distortion of nearly 0.4 mm in radius. This article explains, with figures, how the distortion arises and how to calculate its size, the minimum gripping force that avoids slipping and the centrifugal force, pie jaws and fixtures that hold from the bore, how to split the process, tools and cutting conditions, and how to measure so you do not miss the three lobes. It also includes a calculator that gives the size of the distortion on the spot.

Why it distorts into three lobes: grip, cut, release

① Original shape② Grip: jaws push in, gaps bulge outJaw③ Bore the ID round, still grippedCut here④ Release: inverted 3 lobes in the boreDotted = where the jaws were
Distortion of a thin-wall ring gripped in a 3-jaw chuck (exaggerated; the shape is calculated with the thin-ring formula). Gripping moves the jaw areas inward and the areas between the jaws outward (②). Even if the bore is cut perfectly round in that state (③), the ring tries to spring back once released, so the cut bore ends up with an inverted three-lobe shape, bulging where the jaws were (④)[1][2].

When you grip a low-rigidity ring or tube in a 3-jaw chuck, the areas under the jaws are pushed inward and the areas between the jaws bulge outward. Even if you cut it round in that state, the part tries to return to its original shape on release, so the cut surface is left with a three-lobe shape that is the reverse of the gripped shape. When the bore is cut, the wall is thinnest at the jaw positions, and the cut inner surface distorts more than the outer surface[1][2].

Görög et al. clamped steel tubes (S355J2H; φ89×16, φ70×17.5 and φ70×10.5, length 60 mm) in a 3-jaw chuck at torques of 100, 130 and 160 N·m, bored the inside, and then measured 18 sections on a roundness tester. The results are as follows[1].

  • Roundness is worst at the chuck-side end, and improves with distance from that end
  • The shape is triangular (three lobes) as its main component
  • The thinner the wall, and the higher the clamping torque, the worse the roundness
  • Variation in the ungripped part is small; the effect of distortion is limited to the gripped part

How much it distorts: calculating a thin ring

3-jawRoundness ratio 1 (base)4-jawRoundness ratio 0.286-jawRoundness ratio 0.05
Shapes with the same total gripping force and only the number of jaws changed (all three exaggerated at the same scale). Taking the 3-jaw as 1, the 4-jaw gives about 0.28 and the 6-jaw about 0.05 (theoretical calculation, point contact, elastic)[2].

If you treat the ring as a curved beam, the distortion under equally spaced jaws pressing from outside can be written as formulas. The symbols are: mean radius R (= (OD − wall) ÷ 2), wall thickness t, width b, Young's modulus E, second moment of area I = b × t³ ÷ 12, force per jaw P, number of jaws n, and α = π ÷ n.

  • Compressive force in the section: N₀ = P ÷ (2 sin α)
  • Bending moment at a jaw: M_A = (P × R ÷ 2) × (1/α − 1/tan α)
  • Bending moment midway between jaws: M_B = (P × R ÷ 2) × (1/sin α − 1/α)
  • Radial change (inward is +, θ is the angle measured from a jaw): w(θ) = n × P × R³ ÷ (π × E × I) × Σ cos(k n θ) ÷ ((k n)² − 1)² (k = 1, 2, 3 …)

This formula is based on classical curved-beam theory (inextensible thin-walled ring, point contact, no friction, elastic) and is our own derivation. We therefore ran two checks. First, it matches the classical value for a load at two points (the diameter shrinks by 0.1488 PR³/EI). Second, for the example in the paper by Estrems et al. (an aluminum ring of φ80, 4.5 mm wall and 10 mm width gripped with 930 N per jaw, giving a compressive force in the section of −536 N, a bending moment between the jaws of 3.48 N·m and −6.62 N·m at the jaw position), this formula gives 537 N, 3.48 N·m and 6.58 N·m, which agree closely[2].

Number of jawsAt the jaws (inward)Between the jaws (outward)Roundness ratio (same total force, 3-jaw = 1)
20.074390.068317.09
30.015940.014261.00
40.006080.005390.28
60.001680.001480.052
80.000690.000610.016
120.000200.000180.003

The 2nd and 3rd columns of the table are coefficients to multiply by PR³/EI. As a worked example, take an aluminum ring of φ100 OD, 2 mm wall and 20 mm width (E = 70 GPa, R = 49 mm, I = 13.3 mm⁴). Gripped with a total of 300 N in a 3-jaw chuck (100 N per jaw), it moves inward by 0.20 mm at the jaws and outward by 0.18 mm between them, giving a roundness (radial difference) of about 0.38 mm, and a bending stress at the jaw position of about 69 MPa. The same 300 N on a 4-jaw chuck gives 0.11 mm, and on a 6-jaw chuck 0.020 mm. With a 10 mm width the distortion doubles (0.76 mm with a 3-jaw chuck). Applying a total of 1,000 N with a 3-jaw chuck gives, by calculation, 1.3 mm and 231 MPa, which is near or above the yield strength of aluminum alloy, so the elastic formula no longer holds (the ring is crushed)[2][30].

With point contact from a 3-jaw chuck, a φ100×2 ring distorts even when gripped "gently"As explained later, the gripping force needed for finishing is estimated at about 150 N in total, but with point contact from a 3-jaw chuck the ring still distorts by about 0.19 mm by calculation. You need an approach that spreads the force widely, such as widening the contact angle of the jaws, adding jaws, or holding from the bore.

Calculator: find the distortion when gripped

Enter the OD, wall thickness, width, material, total gripping force and number of jaws, and it gives the radial change at the jaws and between them, a roundness estimate and the bending stress at the jaws, and draws the distortion exaggerated. The error left after release is roughly the inverse of this roundness. If you enter the yield strength, it warns you when the bending stress exceeds it.

Mean radius R = (D − t) ÷ 2; second moment of area I = b × t³ ÷ 12; force per jaw P = F ÷ n; α = π ÷ n (n = number of jaws) Radial change w(θ) = n × P × R³ ÷ (π × E × I) × Σ cos(k × n × θ) ÷ ((k × n)² − 1)² (inward is +) Bending moment at a jaw M = (P × R ÷ 2) × (1/α − 1/tan α); bending stress σ = M × (t ÷ 2) ÷ I

A theoretical estimateThis is an idealized calculation: point contact, no friction, and a material within its elastic range. Actual distortion varies with how the jaws touch (gaps left from forming), the part's initial roundness and wall-thickness variation, and cutting force. Always make a trial cut, release the part and measure its roundness to confirm.

Deciding the gripping force: the minimum to avoid slipping, and centrifugal force

0408012016001,0002,0003,0004,000At rest112 kN74 kNOD grip: falls with speedID grip: rises with speed (concept)Spindle speed (min⁻¹)Gripping force (kN)
SMW-AUTOBLOK example (215 APD-3, standard soft jaws). Centrifugal force rises with the square of the speed, so gripping force falls with OD gripping. With ID gripping it rises instead (the blue dotted line is a concept line that adds the same centrifugal force)[3].

For thin walls you want the gripping force as low as possible, but if it is too low the workpiece slips in the jaws[2]. So we estimate the "minimum force that avoids slipping" by calculation. The formulas in chuck manuals are as follows.

  • Total gripping force is the sum of the radial forces of the individual jaws (10 kN per jaw gives 30 kN for a 3-jaw chuck)[9]
  • Static gripping force = draw force × factor K. For the SMW 210 BHD-3, K = 110 kN ÷ 38 kN ≈ 2.9, so a draw force of 30 kN gives about 87 kN. K is the value for a new, cleaned chuck with the specified grease, so when the grease runs out the gripping force drops even at the same hydraulic pressure[3]
  • Centrifugal force = (master jaw mass × centroid radius + top jaw mass × centroid radius) × number of jaws × ω² (ω = π × speed ÷ 30). The effective centrifugal force measured is about 0.7 times the theoretical value. In the example in the figure above, at 4,000 min⁻¹ the theoretical value is 53.7 kN and the effective value is 38 kN, and the gripping force goes from 112 to 74 kN[3]
  • Required gripping force (Röhm form) = main cutting force × (machining diameter ÷ gripping diameter) × safety factor ÷ friction coefficient. Main cutting force = feed × depth of cut × specific cutting force[5]

In Röhm's worked example, C45 is gripped at a 60 mm gripping diameter and cut at a 20 mm machining diameter with 0.5 mm feed, 5 mm depth of cut and a specific cutting force of 2.50 kN/mm². The main cutting force is 6.25 kN, and with a safety factor of 2.0 and a friction coefficient of 0.20 the required gripping force is about 21 kN. They add the 18 kN loss from centrifugal force at 3,000 min⁻¹, multiply by a further 1.5, and arrive at a gripping force at rest of 58.5 kN[5]. SCHUNK's manual uses the same form (VDI 3106) and says the centrifugal force should be kept to 67% or less of the initial gripping force (DIN EN 1550)[4]. Kitagawa's instruction manual is said to define the maximum permissible speed as the speed at which the dynamic gripping force falls to about 1/3 of the maximum static gripping force[7].

For thin-wall finishing, the main cutting force is far smaller. In the finishing of the aluminum ring by Estrems et al. (feed 0.1 mm, depth of cut 0.5 mm, specific cutting force taken as 300 N/mm²), the main cutting force was 15 N[2]. Applying this to the Röhm form (machining diameter ≈ gripping diameter, safety factor 2, friction coefficient 0.2), the gripping force needed at rest is about 150 N in total (excluding centrifugal force; our calculation). That is at least two orders of magnitude below the tens of kN a power chuck can produce, so it turns out that for thin-wall finishing, even a much-reduced chuck pressure can still be too strong. The reliable way is to measure the actual force with a gripping force meter and decide from that[3][9].

Lighter jaws mean less centrifugal forceCentrifugal force is proportional to the jaw's "mass × centroid radius," so lighter jaws change the gripping force less with rotation. Aluminum soft jaws are sold on this point. For heavy special jaws or jaws mounted outward, SMW cautions you to recalculate and lower the speed[3].

Spreading the force: pie jaws and chucks with more jaws

Standard 3-jaw: 3 pointsForce concentrated at 3 spotsPie jaws: nearly full contactForce spread widely
Left: a standard 3-jaw chuck whose narrow jaws grip at 3 points. Right: pie jaws (wrap-around jaws) that surround and grip almost the whole circumference (illustration; both seen from the front)[1][12].

Pie jaws (wrap-around jaws, as in a segment chuck) have a large contact surface in the circumferential direction to spread the pressure, and are sold for reducing distortion of thin-wall and fragile parts[1][12]. Another approach is to add jaws, such as 12-jaw chucks in which adjacent jaws are linked to press evenly, and chucks with 8 independently moving fingers[11][10]. In a hard-turning example on a hardened (60–64 HRC) bearing race of about 2.25 in OD, a stepped chuck used at minimum pressure improved roundness by 1.35×, versus 10.9× for a chuck whose fingers conform to the shape (a case provided by the manufacturer)[10].

1.00Point0.8930°0.6360°0.3090°0.19100°0.09110°0.04115°0120°Contact angle per jaw (3-jaw; point contact = 1)
Roundness ratio as the jaw contact angle widens (3-jaw; our calculation, assuming the jaws fit the part exactly and the pressure is uniform). At 120° the whole circumference is pressed uniformly and no bending occurs.

In theory, the ratio falls to about 0.30 of point contact at a 90° contact angle and to about 0.09 at 110°. But these are values for the ideal of uniform pressure, and real pie jaws drift toward point contact because of gaps and misalignment from forming. Think of the effect of pie jaws as being decided by how well the forming in the next section is done.

Forming soft jaws: bore them at the gripping diameter and pressure

Grip a forming plug/ringand cut the jawsTool cuts the jaw facesto the workpiece diameter
Illustration of forming soft jaws. With a forming plug (or ring) gripped by the jaws, the gripping faces of the jaws are cut with a tool (part positions are not exact).[8][6].
  1. Prepare a forming toolUse a forming plug for OD gripping and a forming ring for ID gripping. Clean surfaces, no distortion, constant wall thickness. Keep several diameters on hand[8].
  2. Grip near mid-strokeChoose a plug/ring diameter that grips around the middle of the jaws' maximum stroke. Gripping at the end of travel leaves no room for the jaws to move during machining[8].
  3. Seat it, then cutGrip the plug pressed against the chuck face so it does not tilt, re-grip it to seat it, and then cut the step that will hold the workpiece. Use the same hydraulic pressure for forming as for machining, or a little higher[6].
  4. Check with a trial cutRemove the plug, grip the workpiece, and check accuracy and slipping with a trial cut[6].
Formed dia. < workpiece dia.2 points at the ends (6 with 3 jaws)Formed dia. > workpiece dia.1 point at the center (3 with 3 jaws)Formed dia. = workpiece dia.Surface contact
Schematic of one jaw seen from above (gaps exaggerated). Where it touches changes with whether the formed diameter is larger or smaller than the workpiece diameter. Red marks the contact.

If the formed diameter is smaller than the workpiece, contact is at the 2 points at the ends of the jaw (6 points with 3 jaws); if it is larger, contact is at the 1 point in the middle of the jaw (3 points with 3 jaws). One-point contact at the center produces the same distortion as a point-contact 3-jaw chuck, even with pie jaws. As for how far to offset the formed diameter from the workpiece diameter, we found no standard value in the manufacturer documents we reviewed. For thin walls, "forming exactly to the workpiece diameter at the low pressure used for finishing" is logical (because the jaw's own deflection is then cut in the same state), but we have not confirmed a primary source that states this.

Holding by the bore or pressing on the end face: other methods

Spindle (chuck) sideThin-wall sleeve (workpiece)Split sleeve (mandrel)Expands from insideTailstock centerSteadies the endTurn the OD
A thin-wall sleeve held by a mandrel that expands from inside (the yellow split sleeve), supported by the tailstock center while the OD is turned (illustration; cross-section)[13][14].

Instead of pressing from outside with jaws, supporting the part with a mandrel that is inserted in the bore and expanded holds the whole circumference evenly from inside. It is used to locate and hold thin-wall parts by the bore and avoid distortion during precision machining, and is said to allow rings of constant wall thickness[13][14][1]. With ID gripping the gripping force rises with rotation, so take care not to over-expand at high speed.[3].

MethodWhy it worksWeak points / what to check
Pie jaws / full-circumference jawsA wide contact surface spreads the forceReverts to point contact if the forming is poor
Chucks with more jawsLess distortion for the same total force (about 1/19 of a 3-jaw chuck with 6 jaws, in theory)Needs a dedicated chuck[11]
Expanding mandrel / colletSupports the full circumference from inside. Suited to turning the ODThe bore must be finished first[13]
Vacuum chuckHolds by suction on the end face, with no radial pushHolding force = pressure difference × area, capped at atmospheric pressure (about 0.1 MPa). Even over the full face of φ100, theoretically about 785 N (our calculation). Drops with leakage[15]
MagnetThere is a patent for centering with the jaws only and holding the end face with a magnetMagnetic materials only[16]
Low-melting alloy / waxUsed as a material to hold the part temporarily during finishingNo numerical case for thin-wall rings on a lathe was found[17]
Sacrificial grip stock / inner fillerLeave a long gripping section and cut it off at the end / insert a filler inside to support the partA method known in the field; no primary source found to back it
Tailstock / steady restSupports the tip to stop deflectionThere is research (on solid stock) showing that the supporting force greatly changes roundness[21]

Splitting the process: rough, relieve stress, finish

Rough turningHigher pressureRelieve stressTempering, etc.Semi-finishLeave stockFinishingLow pressureRelease and measureafter cooling
Do not rough and finish in one grip: relieve stress in between, and re-grip at low pressure for finishing[18][1].

Rough turning removes a lot of material, produces heat, and changes the balance of stress inside the material. If you finish in the same grip, the shape changes after release. There is a patent in which ring-shaped thin-wall parts are cut in the order rough turning → stress-relief tempering → semi-finishing → finishing (patented)[18], and the commentary on DMG MORI's machining contest also says that choosing the process sequence is the key to preventing out-of-tolerance parts caused by distortion of thin sections[20].

According to a paper summarizing research on bearing rings (secondary citation), boring with a 3-jaw chuck produces a triangular error, and if the OD is then turned with pie jaws, the error of the inner surface is transferred in reverse to the outer surface. Because boring reduces the wall thickness, the gripping force must be lowered when turning the OD. Offsetting the gripping angle between the bore and the OD by 60° minimizes wall-thickness variation but gives the worst roundness[1]. There is also a patent saying that raising the initial gripping force by the amount of the centrifugal force is unsuitable for easily deformed workpieces[19]. If you turn at high speed, consider lowering the speed before raising the pressure.

Tools and cutting conditions: cut without pushing the wall

Small nose radius (R ≤ depth of cut)FeedThin wallLayer being cutForce mainly axialLarge nose radius (R > depth of cut)FeedThin wallLayer being cutPushes the wall radially
Schematic of the idea (cross-section containing the axis). When the nose radius is larger than the depth of cut, only the rounded part of the edge (red) is in contact, and the force tilts toward the radial direction (radial/thrust force) and pushes the thin wall[22][23].

On a thin wall, the radial force (thrust force) pushes directly on the wall, distorts it, and also causes chatter. Here is how to choose tools so as not to push the wall, based on tool-maker documents.

Keep the nose radius smallThe larger the corner radius, the longer the contact with the workpiece and the larger the radial force, so chatter is more likely (Sumitomo Electric). Keep the nose radius equal to or smaller than the depth of cut, and use a smaller radius if chatter occurs (Sandvik)[22][23].
Sharp-cutting edgeA larger positive rake angle lowers cutting force. A wider land or larger honing raises it. Chip breakers that restrain the chip strongly increase the force, so choose one with weak restraint (Tungaloy)[26]. Kyocera's catalog has a category of "sharp-cutting" breakers for thin-wall workpieces[27].
Approach angle near 90°In boring, keep the approach angle as close to 90° as possible and never below 75° (a smaller angle sharply increases the radial force)[24]. A larger approach angle moves the resultant force away from the direction that bends the part[25].
Do not lower the feed too muchCutting force P (kN) = specific cutting force × depth of cut × feed ÷ 1,000. But the smaller the feed, the larger the specific cutting force[22]. A feed so small that the tool only rubs causes heat and chatter.

A Japan Society of Mechanical Engineers conference paper reports that cutting a thin-wall cylinder can cause chatter vibration in which the round cross-section of the workpiece itself deforms[28]. For how to recognize chatter and choose a spindle speed, see Chatter troubleshooting and Chatter speed calculator. The order of fixes and an interactive stability lobe chart are in our chatter decision flow.

Heat and dimensions: just after cutting vs. after cooling

010203040500510152023.5 µm at 10 °CAluminum (23.5 × 10⁻⁶/°C)Steel (12.1 × 10⁻⁶/°C)Temperature difference at measurement (°C)Diameter difference at φ100 (µm)
How much larger the diameter reads when a φ100 part is measured while still warm (coefficients of linear expansion from the UACJ technical report and the Japan Aluminium Association; the diameter difference is our calculation)[29][30].

The coefficient of linear expansion of aluminum is about 23.5 × 10⁻⁶/°C, about twice that of iron (about 12.1 × 10⁻⁶/°C)[29][30]. A φ100 aluminum ring measured while 10 °C warm reads about 23.5 µm larger in diameter (about 12 µm at 5 °C, about 47 µm at 20 °C). Thin-wall parts hold heat poorly, but they warm up quickly from cutting heat and cool quickly too. Measure the finished size after the part has cooled, at the same temperature every time, and equalize the temperature of the part and the cutting fluid before finishing; both matter. To convert between temperature and size, use the The thermal expansion calculator.

How to measure: a micrometer cannot see three lobes

Same diameter in every direction2-point (micrometer)3 lobes read as 0Rotate60° V-block + dialReads 3 lobes ×3 (ellipse = 0)
A three-lobe shape (exaggerated). A diameter measured at 2 points is the same in every direction, so a micrometer reads it as round. Set on a 60° V-block and rotated, the dial indicator reads the three lobes magnified 3×[31][32].

The 2-point diameter method works for even numbers of lobes such as an ellipse, but with an odd number of lobes the side opposite a lobe is a flat, so even a three-lobe workpiece reads as round. The distortion from a 3-jaw chuck is not found by measuring the OD with a micrometer[31][32]. What lets it escape is the 2-point measurement, not the V-block. Set on a V-block and rotated, the lobes are read magnified according to the number of lobes and the V angle. The V opening angle that suits n lobes is 180° − 360° ÷ n: 60° for 3 lobes (reads 3.00×) and 108° for 5 lobes (2.24×)[32].

Measurement2 lobes3 lobes4 lobes5 lobes6 lobes
2-point (micrometer)20202
60° V-block03.00003.00
90° V-block1.002.000.412.001.00
120° V-block1.581.000.422.000.15

The table shows how many times larger than the roundness (radial difference) the reading comes out (V-block values are calculated with the formula we derived, and agree with the Machinery’s Handbook table: 3 lobes at 60° 3.00, 5 lobes at 108° 2.24, 7 lobes at 128.57° 2.11)[32]. The 3 lobes from a 3-jaw chuck read about 2× on a 90° V and 3× on a 60° V. On the other hand, a 60° V reads an ellipse (2 lobes) as 0, and even numbers of lobes are easily hidden by a V-block, so combining 2-point measurement with a V-block reduces the chance of missing them[31]. To evaluate the amount correctly, use a roundness tester (minimum zone method, etc.); Görög et al. also measured 3,600 points per section[1].

Do not measure while still clampedA surface cut while clamped is round as long as it stays clamped. Even if it measures well on the machine, the three lobes appear after release. Measure the part after releasing it and letting it cool.

FAQ

Why can't I assemble a ring turned in a 3-jaw chuck even though a micrometer says it is round?
If you cut while the ring is gripped and distorted in a 3-jaw chuck, a three-lobe shape remains after release. Three lobes (an odd number of lobes) give the same diameter in every direction when measured at 2 points, so a micrometer makes it look round. Check with a V-block (3× for 60°, about 2× for 90°) or a roundness tester.[31][32].
How much better is a 6-jaw chuck?
With the same total gripping force, the point-contact theoretical calculation gives a roundness of about 0.28 times that of a 3-jaw chuck for a 4-jaw chuck and about 0.05 times (about 1/19) for a 6-jaw chuck. This assumes the jaws all touch evenly, so the real improvement can be smaller.[2].
At what pressure should soft jaws be formed?
Kitagawa's instruction manual says the hydraulic pressure for forming should be the same as for machining or slightly higher. When you lower the pressure for thin-wall finishing, forming at that finishing pressure is logical because the jaw deflection is then cut in the same state, but we could not confirm a primary source that states this.[6].
What nose radius should I use for thin-wall finishing?
There is no fixed value, but the tool makers' guideline is a nose radius equal to or smaller than the depth of cut, and smaller still if chatter occurs. The larger the radius, the more radial force pushes on the thin wall.[23][22].

For turning speed and feed, see the turning calculator, for boring see the boring calculator, for thin-wall deflection troubles see Wall deflection, for out-of-size parts see Dimension errors, for measuring tools see Outside micrometer / V-block, for measurement mistakes see Measurement errors, and for NC lathe basics see CNC Lathe Programming for Beginners.

Sources

  1. A. Görög, I. Görögová, Research Papers Faculty of Materials Science and Technology STU 26(42) (2018) DOI 10.2478/rput-2018-0005 (boring of steel tubes held in a 3-jaw chuck, and roundness)
  2. M. Estrems, M. Arizmendi, A. Zabaleta, A. Gil, Procedia Engineering 132, 872-879 (2015) (calculation and experiment on the deformation of a thin-wall ring held in a 3-jaw chuck)
  3. SMW-AUTOBLOK power chuck AP-D instruction manual (calculation of gripping force, centrifugal force and transmissible torque)
  4. SCHUNK ROTA-G instruction manual (gripping force calculation per VDI 3106)
  5. Röhm RN 1391 instruction manual (worked example of required gripping force)
  6. Kitagawa BB200 series instruction manual (forming soft jaws)
  7. Kitagawa BBT200 instruction manual (speed and gripping force)
  8. SAMCHULLY QJC instruction manual (forming plug and forming ring)
  9. TAC Rockford, "Technical Note: Understanding Chuck Forces"
  10. Modern Machine Shop, "Chuck Helps Restore Thin-Walled Hardened Parts to Roundness"
  11. ITW Workholding 12-jaw chuck product introduction (DirectIndustry)
  12. Protool "Aluminum pie jaws for FW" product page
  13. HAINBUCH, "Mandrel MANDO"
  14. Modern Machine Shop, "Expanding the Expanding Mandrel’s Usefulness"
  15. Joe Woodworker "Vacuum Chucking" (holding force = pressure difference × area)
  16. Patent JP5221663B2 (chucking method for workpieces sensitive to deformation and distortion)
  17. Indium Corporation "Low-Temperature Fusible Alloys"
  18. Chinese patent CN118951623B (machining process for ring-shaped thin-wall parts)
  19. US patent US 4,414,871 (chuck gripping force and centrifugal force)
  20. DMG MORI "Cutting Dream Contest" commentary
  21. Nihon University College of Science and Technology, Dept. of Mechanical Engineering, research material (tailstock support force and roundness)
  22. Sumitomo Electric Hardmetal general catalog "Technical Guidance: Turning"
  23. Sandvik Coromant, "How to choose the correct turning insert"
  24. Sandvik Coromant boring tool catalog
  25. Sandvik Coromant, "How to use CoroTurn 107"
  26. Tungaloy "Basics of Chip Breakers"
  27. Kyocera cutting tools general catalog 2024-2026 (turning inserts)
  28. Japan Society of Mechanical Engineers, Dynamics and Design Conference 2019 presentation (chatter vibration in cutting thin-wall cylinders)
  29. UACJ Technical Reports Vol.11 No.1 (2024)
  30. Japan Aluminium Association "Physical Properties of Aluminium"
  31. G. Schuetz (Mahr) "Determining Out-of-Roundness at the Point of Manufacture" Modern Machine Shop (2022)
  32. Machinery’s Handbook 31st edition (measuring roundness with V-blocks)

More articles