Printed from Kezuriba (kezuriba.net/en/materials/sk105/)
SK105
ISO P (steel)Carbon tool steels. Standard: JIS G 4401 (The current edition appears to be JIS G 4401:2025).
International equivalents
“Close” means composition or properties are not exactly the same. Before substituting, check the values in each standard.
| System | Designation | Number | Relation | Confidence |
|---|---|---|---|---|
| JIS | SK105 | JIS G 4401 | — | |
| AISI | W1 | close | Agrees in 2+ sources[4][6][7] | |
| EN | C105W1designation of the former DIN 17350 | 1.1545 | close | Agrees in 2+ sources[6][4] |
| GB | T11carbon tool steel in GB/T 1299 tool and die steels | close | One source / reference[4] |
Differences between the equivalents (from the sources)
- AISI W1: Kyocera's comparison table assigns "W1-10" (apparently meaning W1 with about 1.0% C) to SK105 (SK3), and Mitsubishi Materials' comparison table assigns W1 to SK3. In Proterial's AISI comparison table, W1 is a broad standard with C 0.60–1.40, and the JIS column is blank. The UNS number could not be confirmed in primary sources
- EN C105W1: Mitsubishi Materials' cross-reference table assigns W-Nr. 1.1545 and DIN C105W1 to SK3, and Kyocera's table also gives C105W1 in the DIN column (the number 1.1545 appears only in Mitsubishi Materials). The designation in the current EN ISO 4957 (often said to be C105U) is not confirmed in primary sources. Kyocera gives C105E2U in the French NF column
- GB T11: Kyocera's cross-reference table only. The same table has SK120 = T12 and SK95 = T10, arranged in order of C content. Mitsubishi Materials' table has an empty GB column. The GB-side composition is not confirmed in primary sources
Chemical composition (mass %)
As specified in JIS G 4401 (Kobe Steel standard table [5-1) G 4401 Carbon tool steels, 2009 revision], row of YK3 [equivalent JIS designation SK105] in the Daido YK30 catalog)
| Element | Range | Confidence |
|---|---|---|
| C | 1.0 – 1.1 | Agrees in 2+ sources[1][2] |
| Si | 0.10 – 0.35 | Agrees in 2+ sources[1][2] |
| Mn | 0.1 – 0.5 | Agrees in 2+ sources[1][2] |
| P | ≤ 0.03 | Agrees in 2+ sources[1][2] |
| S | ≤ 0.03 | Agrees in 2+ sources[1][2] |
| Cu | ≤ 0.25 | Agrees in 2+ sources[1][2] |
| Ni | ≤ 0.25 | Agrees in 2+ sources[1][2] |
| Cr | ≤ 0.3 | Agrees in 2+ sources[1][2] |
Density
—
Not confirmed
No primary source giving the density of SK105 itself, or of EN 1.1545, was found
The density could not be confirmed. In the weight calculator, use “Steel, general value” or enter your own.
Material cost comparison: Metal and plastic price guide.
Mechanical properties
“Reference” values are not specified minimums from the standard but figures published by makers and others.
| Condition | Tensile MPa | Yield MPa | Elong. % | Hardness | Type of value |
|---|---|---|---|---|---|
| Annealed | — | — | — | — | No primary source was found that gives the JIS specified value (annealed hardness). Kobe Steel's table gives composition only, and the Aichi Steel page does not state the hardness of SK3 Not confirmed |
| Quenched and tempered (water quenched) | — | — | — | — | No primary source giving JIS specified values (quenching and tempering temperatures and hardness) was found. The Daido YK30 catalog gives only the quenching test conditions for YK3, and hardness is shown only in graphs, not as numerical values Not confirmed |
1 MPa ≈ 145 psi (0.145 ksi). Hardness conversion · unit converter
Machinability notes (as stated in the sources)
- Sandvik Coromant shows the high-carbon (C >0.55%) group of unalloyed steels with examples of 190 HB annealed (specific cutting force kc1 1750 N/mm²) and 300 HB quenched and tempered (kc1 2000 N/mm²), and states that the higher the C, the greater the hardness and abrasive wear of the cutting edge. These are not values that name SK105[5]
- Proterial Special Steel explains that SK steels, which contain no alloying elements, have poor hardenability and can only be water quenched, and that SKS93 and SKS3, with small additions of Mn and Cr, can be oil quenched. Aichi Steel describes SK3 as a general-purpose carbon tool steel[8][3]
Frequently asked questions about SK105
- What are the international equivalent grades (JIS, ASTM, SAE, EN, ISO, GB) for SK105?
- Comparable grades to SK105 (Carbon tool steels) include W1, C105W1, T11. Because composition limits and mechanical property ranges differ slightly between standards, verify the exact table values above before substituting on a drawing.
- What is the ISO material group and specific cutting force (kc1) of SK105?
- SK105 belongs to ISO material group P (steel). Select insert grades and chipbreakers rated for ISO P.
- What is the most important precaution when machining SK105?
- Sandvik Coromant shows the high-carbon (C >0.55%) group of unalloyed steels with examples of 190 HB annealed (specific cutting force kc1 1750 N/mm²) and 300 HB quenched and tempered (kc1 2000 N/mm²), and states that the higher the C, the greater the hardness and abrasive wear of the cutting edge. These are not values that name SK105
Sources
Primary sources (public documents from makers, industry associations and standards bodies), numbered where each value is cited. Many are in Japanese.
- kobelco.co.jp https://www.kobelco.co.jp/products/steel-aluminum/wirerod/pdf/202012_wirerod_standard.pdf
- daido.co.jp https://www.daido.co.jp/common/pdf/pages/products/tool/yk30.pdf
- aichi-steel.co.jp https://aichi-steel.co.jp/ENGLISH/products/hagane_company/tool_steel/cold/
- kyocera.co.jp https://www.kyocera.co.jp/prdct/tool/wp-content/uploads/2016/06/R_2016.pdf
- sandvik.coromant.com https://www.sandvik.coromant.com/en-us/knowledge/materials/workpiece-materials
- data.mmc-carbide.com https://data.mmc-carbide.com/5916/5780/3641/tec_metalic_materials_xref_ja.pdf
- proterial.com https://www.proterial.com/products/tool_steel/techinfo/coldforging/05.html
- ss.proterial.com https://www.ss.proterial.com/zatsugaku/property.html