Printed from Kezuriba (kezuriba.net/en/materials/sum24l/)
SUM24L
ISO P (steel)Sulfur and sulfur-composite free-cutting steels (low-carbon composite free-cutting steel with added lead). Standard: JIS G 4804 (JIS G 4804:2008).
International equivalents
“Close” means composition or properties are not exactly the same. Before substituting, check the values in each standard.
| System | Designation | Number | Relation | Confidence |
|---|---|---|---|---|
| JIS | SUM24L | JIS G 4804 | — | |
| AISI/SAE | 12L14 | equivalent | Agrees in 2+ sources[3][10][7][8][11] | |
| EN | 9SMnPb28old DIN designation | 1.0718 | close | One source / reference[3][11] |
| NF | S250Pb | close | One source / reference[3][11] | |
| GB | Y15Pb | close | One source / reference[3] |
Differences between the equivalents (from the sources)
- AISI/SAE 12L14: Kyocera's metal material symbol cross-reference table places SUM24L and 12L14 in the same row. JFE's English technical report (No.15) writes "AISI12L14 (JIS SUM24L)", and JFE Technical Report No.55 writes "AISI 12L14, JIS SUM24L (0.10–0.35% Pb)", treating them as the same grade. On the other hand, Mitsubishi Materials' cross-reference table (Russian version) places 12L14 in the 1.0737 9SMnPb36 row, with "–" (no equivalent) in the JIS column. The composition range in the SAE standard text and the UNS number (said to be G12144) are not confirmed in primary sources. The analysis examples are close: Nippon Steel Corporation's SUM 24L is C 0.08, Mn 1.1, P 0.075, S 0.32, Pb 0.28; JFE's 12L14 is C 0.06, Mn 1.0, P 0.06, S 0.32, Cr 0.1, Pb 0.26
- EN 9SMnPb28: Kyocera's comparison table lists 9SMnPb28 in the DIN column for SUM24L. The material number 1.0718 is the value in Mitsubishi Materials' comparison table. However, Mitsubishi matches 1.0718 9SMnPb28 to SUM22L and 12L13, and 1.0737 9SMnPb36 to 12L14, so the sources disagree. The current EN 10087 designations (such as 11SMnPb30) and the EN composition ranges have not been confirmed in primary sources
- NF S250Pb: NF column of Kyocera's comparison table. In Mitsubishi's comparison table, S250Pb is in the row of 1.0718 9SMnPb28, and the 12L14 row (1.0737) is S300Pb
- GB Y15Pb: GB column of Kyocera's comparison table only. The GB standard number and composition could not be obtained from primary sources, so no comparison was made. In Mitsubishi's comparison table the GB column of the 12L14 row is "-"
Chemical composition (mass %)
As specified in JIS G 4804
| Element | Range | Confidence |
|---|---|---|
| C | ≤ 0.15 | One source / reference[1] |
| Si | Not specified (limits or ranges such as 0.10% max., 0.10-0.20%, or 0.15-0.35% may be set by agreement between the parties to the delivery) | Agrees in 2+ sources[1][2] |
| Mn | 0.85 – 1.15 | One source / reference[1] |
| P | 0.04 – 0.09 | One source / reference[1] |
| S | 0.26 – 0.35 | One source / reference[1] |
| Pb | 0.10 – 0.35 | Agrees in 2+ sources[1][7] |
Density
7.85 g/cm³
One source / reference[9]
Value from Sanyo Special Steel's "steel weight table (kg/m) (specific gravity 7.85)". It is the general value for steel used to calculate bar mass, not specific to SUM24L. The density of SUM24L itself, which contains 0.10-0.35% lead, was not found in primary sources
Calculate weight in SUM24L →Material cost comparison: Metal and plastic price guide.
Mechanical properties
“Reference” values are not specified minimums from the standard but figures published by makers and others.
| Condition | Tensile MPa | Yield MPa | Elong. % | Hardness | Type of value |
|---|---|---|---|---|---|
| Test material (condition not stated; the SUM 24L used in machinability tests) | — | — | — | HV 113 | Measured example (Nippon Steel Technical Report No. 386, Table 2; SUM 23 in the same test was also HV 113; not a specified value) One source / reference[8] |
| Test material (conventional AISI 12L14 steel; condition not stated) | 427 | 284 (0.2% proof strength) | 31.8 | — | Measured example (JFE Technical Report No. 55, Table 2; JFE treats AISI 12L14 and JIS SUM24L as the same steel; not a specified value) One source / reference[7] |
1 MPa ≈ 145 psi (0.145 ksi). Hardness conversion · unit converter
Machinability notes (as stated in the sources)
- Nippon Steel (Nippon Steel & Sumitomo Metal Technical Report No. 406, 2016) describes low-carbon free-cutting steels classified as JIS SUM as steels for office automation equipment and hydraulic parts, where machining accuracy is required more than strength; about 0.3% Pb or S is added for high machinability. Because of the large amount of free-cutting elements, chip disposal is not a problem and finished surface roughness is what matters. In an interrupted-cutting (quick-stop) test of SUM24L, cracks form around the built-up edge starting from MnS (with lead crystallized around it), which suppresses growth of the built-up edge and improves the finished surface[12]
- Nippon Steel Technical Report No. 386 (2007): SUM 24L, which is SUM 23 (sulfur free-cutting steel) with lead added, has better machinability than SUM 23. Lead acts as a lubricant between tool and workpiece in the high-temperature cutting zone and embrittles ferrite, so the built-up edge is shed frequently and its growth is suppressed. In plunge cutting simulating automotive hydraulic parts (800+ pieces), SUM 24L was better than SUM 23 in both surface roughness and tool wear, and its cumulative drilled hole depth was also greater than that of SUM 23. Low-carbon free-cutting steels are common in small parts where oil seal areas, bearing seats, and fits are important[8]
- JFE Technical Report No. 55 (2025): the tool tip exceeds 400 °C during cutting, and Pb, with a melting point of 327 °C, causes liquid metal embrittlement and keeps the built-up edge small. As a result, worsening of surface roughness by the built-up edge and tool wear from a large or detaching built-up edge are suppressed. JFE's English technical report (No. 15) states that 12L14 (SUM24L) is used in large quantities for OA equipment parts such as transmission hydraulic control valves, hydraulic hose fittings, and printer shafts, and that its oxygen content is high, about 150 ppm[7][10]
- Sandvik Coromant classifies free-cutting steel under ISO P (MC code P1.4 "free cutting steel"). Pb in free-cutting steel has a low melting point and lowers friction between chip and insert, and is often added at about 0.25% in combination with S. Low-carbon steels under 0.2% C show more adhesive wear and tend to form a built-up edge, and their chips are also hard to break[5]
Frequently asked questions about SUM24L
- What are the international equivalent grades (JIS, ASTM, SAE, EN, ISO, GB) for SUM24L?
- Comparable grades to SUM24L (Sulfur and sulfur-composite free-cutting steels (low-carbon composite free-cutting steel with added lead)) include 12L14, 9SMnPb28, S250Pb, Y15Pb. Because composition limits and mechanical property ranges differ slightly between standards, verify the exact table values above before substituting on a drawing.
- What is the ISO material group and specific cutting force (kc1) of SUM24L?
- SUM24L belongs to ISO material group P (steel). Select insert grades and chipbreakers rated for ISO P.
- What is the most important precaution when machining SUM24L?
- Nippon Steel (Nippon Steel & Sumitomo Metal Technical Report No. 406, 2016) describes low-carbon free-cutting steels classified as JIS SUM as steels for office automation equipment and hydraulic parts, where machining accuracy is required more than strength; about 0.3% Pb or S is added for high machinability. Because of the large amount of free-cutting elements, chip disposal is not a problem and finished surface roughness is what matters. In an interrupted-cutting (quick-stop) test of SUM24L, cracks form around the built-up edge starting from MnS (with lead crystallized around it), which suppresses growth of the built-up edge and improves the finished surface
Sources
Primary sources (public documents from makers, industry associations and standards bodies), numbered where each value is cited. Many are in Japanese.
- sanyo-steel.co.jp https://www.sanyo-steel.co.jp/product/special_steel/images/pdf/akahon_201906.pdf#page=123
- kobelco.co.jp https://www.kobelco.co.jp/products/steel-aluminum/wirerod/pdf/202012_wirerod_standard.pdf#…
- kyocera.co.jp https://www.kyocera.co.jp/prdct/tool/wp-content/uploads/2016/06/R_2016.pdf#page=14
- jfe-steel.co.jp https://www.jfe-steel.co.jp/products/bousen/catalog/h1j-001.pdf
- sandvik.coromant.com https://www.sandvik.coromant.com/en-us/knowledge/materials/workpiece-materials
- kyocera.co.jp https://www.kyocera.co.jp/prdct/tool/wp-content/uploads/2014/07/2024-2026_A.pdf
- jfe-steel.co.jp https://www.jfe-steel.co.jp/research/giho/055/pdf/055-17.pdf
- nipponsteel.com https://www.nipponsteel.com/tech/report/nsc/pdf/38608.pdf
- sanyo-steel.co.jp https://www.sanyo-steel.co.jp/product/special_steel/images/pdf/akahon_201906.pdf#page=269
- jfe-steel.co.jp https://www.jfe-steel.co.jp/en/research/report/015/pdf/015-04.pdf
- mitsubishicarbide.net https://www.mitsubishicarbide.net/contents/mhg/ru/manual/material_cross_reference.pdf